 AR (Anti-Reflection) Coating by Vacuum Evaporation Method

- Minimizing the reflectance of plastics used for front panel of LCD etc.
- Higher transmittance
Optical Properities (Single Side)
- Low reflectance in wider range of wavelength
- Extremely minimizing the reflection color
Optical Properities (Single Side)
Illuminant D65 - CIE Chromaticity Diagram
- Applicable to non-hard coated materials which enable to obtain adequate adhesiveness without hard coating such as aspherical acrylic lens and cyclo-olefin polymer, copolymer.
Samples : Aspherical Lenses
Physical Properties*
|
UV Resistivity Test
|
|
Conditions
|
|
 |
Xenon light irradiation (1,000 hours)
|
|
 |
Inspected substrate : MR-200 by MITSUBISHI RAYON CO., LTD.
|
|
Results
|
|
 |
Contact angle : 108 degrees
|
|
 |
Adhesion (Tape test) : Passed
|
|
|
Anti-Salt Water AR Coating
|
|
|
|
Corroded surface by salt water
|
Non corroded surface by anti-salt water effect
|
Fishfinder
|
|
Salt Water Spray Test (Salt Water Resistivity Test)
|
|
Conditions
|
|
 |
Per JIS Z2371, 28 days
|
|
 |
Inspected substrate: MR-200 by MITSUBISHI RAYON.CO.LTD.
|
|
Results
|
|
 |
Contact angle : 108 degrees
|
|
 |
Adhesion (Tape test) : Passed
|
The test was conducted by the Nagoya Municipal Industrial Research Institute, using a salt water spray testing machine made by Suga Test Instruments Co, Ltd.
Test conditions: chamber temperature 35 ± 1 °C, approx. 100% humidity, 5% salt water density (50g / 1000ml), PH6.5-7.2
*All of optical and physical properties are not the guaranteed values but the results of the measurement.
**All the NIDEK's coating for optical application are individually designed on a make-to-order basis.
|
|